chilled cast iron roll3

Chilled Cast Iron Roll

Avail this product from Tinvo  as there is no free graphite in the working layer of alloy chilled cast iron roll.

Indefinite Chilled Cast Iron (ICCI) rolls, also known as ICDP rolls, feature a microstructure where graphite flakes are distributed throughout the working layer. Unlike standard chilled rolls, ICCI rolls have no distinct ‘chill line’ between the shell and the core, which is the key to their superior performance.

Introduction

There is no free graphite in the working layer of alloy chilled cast iron roll, it is featured as high hardness, good wear resistance, and micro metallographic micro-structure is fine pearlite and carbides.

Mastery of Chill Depth

Precision Hardness: We maintain strict control over the chill depth (hardened layer) to ensure consistency throughout the roll’s service life. This allows for multiple re-grinds while maintaining the required surface hardness (HSD 60-80)

Exceptional Surface Finish

Mirror-Like Performance: Due to the high density of iron carbides in the chilled layer, our rolls can be polished to an exceptional finish, making them ideal for industries where surface precision is critical, such as paper calendering and metal foil rolling.

Dual-Phase Structure

The ‘Hard Shell, Soft Heart’ Design: The rapid cooling creates a wear-resistant cementite-rich shell, while the slower-cooled core remains grey iron, providing the fracture toughness needed to withstand operational stresses.

Indefinite Chilled (ICDP) Rolls — How They Differ

Superior Anti-Spalling Performance: TINVO’s ICCI rolls are engineered with a unique graded microstructure. Since there is no distinct “chill line” between the working layer and the core, the internal thermal stresses are significantly minimized. This drastically reduces the risk of surface spalling and catastrophic roll failure under high-load conditions.

Minimal Hardness Drop: Our Indefinite Chilled Cast Iron rolls feature an optimized alloy distribution. This ensures that the surface hardness remains consistent throughout the entire service life of the roll, allowing for multiple re-grinds without compromising wear resistance.

Excellent Thermal Crack Resistance: The presence of fine, evenly distributed graphite flakes acts as a natural lubricant and thermal buffer. This characteristic provides the rolls with exceptional resistance to thermal fatigue and “fire-cracking” during rapid heating and cooling cycles in hot rolling stands.

Premium Surface Quality: The sophisticated metallurgical bond between the carbides and the matrix allows for a mirror-like finish after grinding. This ensures that the rolled steel products (strip, bar, or plate) maintain a high-quality surface with minimal imperfections.

As a specialized class within the Chilled Iron Roll family, ICDP / Indefinite Chilled Cast Iron rolls share the high-carbide work layer concept with standard chilled cast iron rolls, but differ in microstructure: the absence of a distinct chill line gives ICDP its characteristic graded transition from work layer to core. For mills comparing the two families in the context of stand selection, see the standard chilled cast iron roll family page for the broader chilled iron roll classification.

No single grade wins on every stand, and the choice between a chilled body and an indefinite chilled one is usually settled by the cooling water rather than by the hardness figure. Where cooling is reliable and abrasive wear dominates, the conventional chilled roll stays the cheaper way to hold a surface; where the stand sees stops and restarts, the graded structure of ICDP earns its price. We set the four materials side by side, stand position by stand position, in our roll material comparison.

Application

The main application of the cast iron rolls are work roll of bar & wire rod mill, hot strip mill, cold strip mill, PC mill, section mill, plate rolling mill, non-ferrous mill, pre-finishing stands of high speed wire, stretch reducing mill for seamless steel tube, etc.

  • Need higher wear resistance for late finishing stands? Check our HSS Rolls.
  • Looking for roughing mill solutions? View our Adamite Rolls.
  • For high-speed finishing stands requiring maximum wear resistance, explore our High NiCr ICDP Rolls.

Chemical Composition

Roll CSiMnPSNiCrMo
Ni-Cr-Mo chilled iron roll(I)3.20~3.700.40~0.800.20~0.50≤0.40≤0.100.50~1.000.20~0.600.20~0.60
Ni-Cr-Mo chilled iron roll(II)3.20~3.700.40~0.800.20~0.50≤0.40≤0.101.01~2.000.30~1.200.20~0.60
Ni-Cr-Mo chilled iron roll(III)3.20~3.700.40~0.800.20~0.50≤0.40≤0.102.01~3.000.50~1.500.20~0.60

Indefinite Chilled Cast Iron Roll

Roll CSiMnPSNiCrMo
Cr-Mo infinite chilled cast iron roll3.20~3.700.80`1.200.60~1.00≤0.20≤0.10/0.60~1.200.20~0.60
Ni-Cr-Mo infinite chilled cast iron roll(I)3.20~3.700.80`1.200.60~1.00≤0.20≤0.100.50~1.000.70~1.200.20~0.60
Ni-Cr-Mo infinite chilled cast iron roll(II)3.20~3.700.60~1.000.60~1.00≤0.20≤0.101.01~2.000.70~1.200.20~0.60
Ni-Cr-Mo infinite chilled cast iron roll(III)3.20~3.700.60~1.000.60~1.00≤0.20≤0.102.01~3.000.70~1.200.20~0.6

Physical Properties

Roll                      Roll-body hardnessRoll-neck hardnessTensile strengthChill depth
Section steel
Ni-Cr-Mo chilled iron roll(I)60~7032~50>150<Φ200Φ201~250Φ251~300>Φ300
Ni-Cr-Mo chilled iron roll(II)62~7535~52>15012~2515~3017~3520~45
Ni-Cr-Mo chilled iron roll(III)65~8040~55>15012~2515~3017~3520~45

Indefinite Chilled Cast Iron Roll

Roll Roll-body hardness HSDRoll-neck hardness HSDTensile strength       Mpa
Cr-Mo infinite chilled cast iron roll55~7035~55>160
Ni-Cr-Mo infinite chilled cast iron roll(I)60~7235~55>160
Ni-Cr-Mo infinite chilled cast iron roll(II)62~7235~55>160
Ni-Cr-Mo infinite chilled cast iron roll(III)65~7535~55>160

Metallographic Structure

RollMetallographic structure
Ni-Cr-Mo chilled iron roll(I)Pearlite + cementite + lai type body
Ni-Cr-Mo chilled iron roll(II )Fine pearlite + cementite + lai type body
Ni-Cr-Mo chilled iron roll(III )Type body + cementite + lai type body

Indefinite Chilled Cast Iron Roll

Roll Metallurgical structure
Cr-Mo infinite chilled cast iron rollPearlite + cementite + a little graphite
Ni-Cr-Mo infinite chilled cast iron roll(I)Pearlite + cementite + a little graphite
Ni-Cr-Mo infinite chilled cast iron roll(II)Fine pearlite + cementite + a small amount of graphite
Ni-Cr-Mo infinite chilled cast iron roll(III)Type body + cementite + a small amount of graphite

Customization

Leave your RFQ and provide the drawings, chemical composition, hardness, physical properties, etc. 

Versatile Industrial Applications: Beyond steel mill stands, TINVO’s chilled rolls are widely trusted in food processing (flour, oilseed) and polymer compounding.

Q: Where is a chilled cast iron roll the right choice?

A: Where abrasive wear governs and the stand tolerates a body that is hard at the surface and relatively inelastic through the section. That is most often a finishing position on a bar, rod or section mill rather than a roughing stand.

Q: What does the chill depth change about roll behaviour?

A: It sets how much usable working layer exists before the softer core is exposed. A deeper controlled chill extends the number of regrinding cycles; an uncontrolled chill line produces an abrupt hardness step that becomes a spalling origin.

Q: How does an ICDP roll differ from a conventional chilled roll?

A: ICDP has no defined chill line. The transition from the white iron working layer to the core is graded rather than abrupt, which is what gives the roll a deeper usable layer and better tolerance of thermal cycling. 

Q: What should the roll specification state?

A: The shell composition range, the chill depth and the hardness profile through it, the core grade, and the minimum permissible diameter at scrapping. The minimum diameter is what converts the working layer into a number of regrind cycles.